Title |
A Study on high Quality of Antiwashout Underwater Concrete
|
Keywords |
heat evolution amount; setting time; suspended solids; efflux time |
Abstract |
In case of constructing concrete structure under water, generally concrete mixed with antiwashout admixture, high range water reducer, or AE-water reducing agent etc has been manufactured to ensure the quality of antiwashout underwater concrete because of being difficulty in ascertaining construction situation by the naked eye. The properties of high quality antiwashout underwater concrete that were aimed at affluent fluidity, workability and the compressive strength of 450 kgf/㎠ at 28 ages using two types of blended cements are following as;(1) Setting time of antiwashout underwater concretes using blended cements was more greatly delayed than that of control concrete, however, was satisfied with criteria value of "Quality standard specification of antiwashout admixture for concrete".(2) As a test results of slump flow, efflux time and box elevation of head, it was found that workability of high quality antiwashout underwater concrete was improved. (3) Heat evolution amount of OPC was 1.5 times as high as that of two types of bended cements in 72 hours. (4) Suspended solids of antiwashout underwater concrete using blended cements was more than that of control concrete, also compressive strength of high quality antiwashout underwater concrete was very low in early age, but was better than that of control concrete as to increasing ages.
|