Title |
A Study on the Influence Factors on Crack Properties of CFRD Face Slab Concrete
|
Keywords |
CFRD; polypropylene fiber; drying shrinage; permeability; plastic shrinkage |
Abstract |
CFRD(Concrete Faced Rockfill Dam) face slab concrete has a much capability to occur crack due to drying shrinkage, plastic shrinkage and bad compaction etc. Because of these cracks of concrete induce structural problem and decrease durability of dam, it is need to reduce crack of face slab concrete. This is an experimental study to analyze the influence factors on crack properties of CFRD face slab concrete. For this purpose, various mix proportion of CFRD face slab concrete and concrete using PPF(polypropylene fiber0 and fly ash was selected. And tests for drying shrinkage, bonding strength, water permeability and plastic shrinkage were performed, and then CFRD D and PPC of those mix proportion were placed in CFRD field. According to test results, it was found that the bonding strength of C1(compact sufficiently) was higher about 10~20% than that of C2(compact insufficiently). And the engineering properties of PPC(concrete using PPF) and FAC(concrete using fly ash) were better than those of the others ; the permeability of PPC and FAC after 8 weeks curing was little lower than that of CFRD D, and plastic shrinkage crack of PPC and FAC was lower 40~60% than crack of CFRD D.
|